The lowest observed group mean is 20.375 for welding method group 2. The highest is 27.442 for group 1, a difference of 7.067 on the source response scale. Across all 24 numeric records the response median is 22.5.
What was measured
The SHEESLE2 data file has 25 header lines before the tabulated area. The header supplies the test context, column order and reading instructions. This analysis uses the column described as average (over 4 reps) of defective leads/hour. It preserves the source scale and its sign. The file contains 6 numeric fields per accepted row.
Spread across the original readings
The two endpoint groups have 12 and 12 observations. Their medians are 21.7 and 27.1, respectively. The figure groups the original entries by the recorded welding method value. Where there are more than eight distinct settings, it groups them at empirical quartiles and labels each band with its observed endpoints.

One row you can check
To check a real observation, take numeric row 22 after the header. Its response is 22.5. The overall arithmetic mean is 23.908, so this observation is -1.408 units from the mean on the original scale. Sorting the whole response gives an interquartile spread of 6.875, calculated by subtracting 20.125 from 27.
The centre and spread are descriptive statistics. Each numeric observation carries the same weight in the overall summary. Treat grouped results as a way to find a measurement difference worth investigating. They do not adjust simultaneously for all factors, run order, sample selection or repeated measurements in the original study.
Worked data
welding method group | Observations | Mean response | Median response | Minimum response | Maximum response |
|---|---|---|---|---|---|
1 | 12 | 27.44167 | 27.1 | 19.9 | 38.2 |
2 | 12 | 20.375 | 21.7 | 12.8 | 26.6 |
Implications for an industrial comparison
Record fixture connections, instrument range, excitation level and temperature alongside the measured result. Repeatability within one setup can remain good even when fixtures differ between laboratories. A useful acceptance run includes both a repeat measurement without disturbing the setup and a repeat after a normal reconnection.
Choose a decision threshold in the engineering units before collecting a local series. Preserve raw readings, any exclusions and a record of the operating conditions so that a later analyst can separate a real change from differences in data handling.
Source file and worked data
The original NIST Dataplot header and measurements include the study attribution. Download the complete source file. Download the worked data used in the figure.
Cover photograph by Peter Xie, via Pexels. The photograph illustrates the subject. Industry Applied produced the figure and calculations from the linked source.